Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-1025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00146 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B40-0039 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B7-19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E21D11-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E02D17-20 |
filingDate |
2005-05-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2008-04-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-WO2005123620-A1 |
titleOfInvention |
Spray setting agent, spraying material, and spraying method using the same |
abstract |
Provided are a quick setting agent capable of imparting high durability and excellent quick setting and strength development while reducing the amount of alkali used, and a spraying method using the quick setting. A spray setting agent containing calcium aluminate, gypsum, and alkali metal aluminate, wherein the calcium aluminate has a vitrification rate of 80% or more and a CaO / Al 2 O 3 molar ratio. 1.9 to 3.0, and the content of the alkali metal aluminate is 1.5 to 10 parts in 100 parts of the spray accelerating agent. Agent. |