http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2005113647-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G73-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K1-0346 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K1-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G73-16 |
filingDate | 2004-11-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2008-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2005113647-A1 |
titleOfInvention | Polyesterimide and its precursor with low linear thermal expansion coefficient |
abstract | INDUSTRIAL APPLICABILITY The present invention has a practically useful polyesterimide, precursor thereof, and production thereof having a low dielectric constant, a low linear thermal expansion coefficient, a high glass transition temperature, and sufficient film toughness for flexible printed wiring board applications. A method is provided. Formula (2): In the formula, A and B are each independently a divalent aromatic group, an alicyclic group, or a combination thereof, provided that all the divalent bond positions relative to adjacent atoms are all A polyesterimide comprising a repeating unit represented by the para-position or a relationship corresponding thereto. |
priorityDate | 2004-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |