http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2005035623-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-912 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-08 |
filingDate | 2004-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2006-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2005035623-A1 |
titleOfInvention | Method for producing aliphatic polyester |
abstract | Improve the water resistance of the aliphatic polyester obtained by actively using water as an initiator or / and molecular weight regulator. More specifically, an aliphatic polyester obtained by ring-opening polymerization of a cyclic ester containing a proton source compound containing water exceeding 80 ppm as an initiator or / and a molecular weight regulator using the total proton concentration in the cyclic ester as an index. Aliphatic polyester is manufactured by mix | blending a carboxyl group sealing agent with this. |