http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2004069923-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K3-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J201-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G81-00 |
filingDate | 2004-01-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2006-05-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2004069923-A1 |
titleOfInvention | Polymer and curable composition having improved storage stability |
abstract | In the composition of a vinyl copolymer having a crosslinkable silyl group, curing may be delayed after storage. (I) A curable composition comprising, as an essential component, a vinyl polymer having at least one crosslinkable silyl group at its terminal and having a monomer containing a methyl ester group as an essential constituent unit. Sealing material, liquid gasket, and adhesive using the curable composition. It has at least one crosslinkable functional group at the end, the main chain is a vinyl polymer, and 2 to 80% of the monomers constituting the main chain are methyl acrylate by weight ratio. A characteristic polymer. The following two components: (A) a vinyl polymer having at least one crosslinkable silyl group, (B) A curable composition having improved storage stability comprising a compound other than (a) having a methyl ester group as an essential component. |
priorityDate | 2003-01-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |