http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2004067625-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2321-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C2009-0021 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L101-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C15-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L101-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-215 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-0016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-0025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-00 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C15-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-215 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 |
filingDate | 2004-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2006-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2004067625-A1 |
titleOfInvention | Diene rubber composition and method for producing the same |
abstract | A diene rubber composition excellent in processability, having excellent pulling strength and wear resistance while achieving both low fuel consumption and high grip properties, a diene rubber obtained by crosslinking the same, and a method for producing the same It is to provide. The composition is characterized by 100 parts by weight of a diene rubber having a molecular weight distribution of 1.1 to 30 expressed by the ratio of the weight average molecular weight to the number average molecular weight, 20 to 200 parts by weight of silica, and a cationic polymer. The amount of the rubber component insoluble in toluene with respect to 1 g of silica is 0.2 g to 1 g, and is a diene-based cross-linked rubber obtained by cross-linking it, and its production characteristics are stabilized by an anionic emulsifier. The rubber latex is reacted with an aqueous suspension of silica containing a cationic polymer to co-coagulate the rubber in the rubber latex and the silica in the aqueous suspension within a specific pH range. |
priorityDate | 2003-01-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 132.