http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2003062299-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G69-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-78 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G69-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-78 |
filingDate | 2003-01-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2005-05-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2003062299-A1 |
titleOfInvention | Method for producing aromatic polymer |
abstract | The present invention is a method for producing a high-quality aromatic polymer by batch-type continuous polymerization, a reaction tank having a raw material supply port and a polymer discharge port, a stirring device, a distillation pipe, a reaction temperature management device, and a reaction pressure management device. When the aromatic raw material is polycondensed to produce an aromatic polymer in a batch system, the temperature of the reactor part in contact with the reaction space is maintained at 150 to 300 ° C. during the polycondensation reaction. The reaction temperature is in the range of 300 to 400 ° C, the temperature is raised from 280 ° C to the final reaction temperature at 0.5 ° C / min or less, and after reaching the final reaction temperature, the internal pressure of the reaction system is reduced to 25 to 200 Torr. Then, polycondensation is performed. |
priorityDate | 2002-01-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |