http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S6395293-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65G53-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10L10-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10L1-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K23-52 |
filingDate | 1986-10-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7db27e79dcc1471da6edf869fbed8b85 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dd64fee2919c7abdfcec86f31c38dcfb |
publicationDate | 1988-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-S6395293-A |
titleOfInvention | Dispersion stabilizer for coal-water slurry system |
abstract | PURPOSE: To obtain a dispersion stabilizer providing coal-water slurry having excellent fluidity and stability at high coal concentration, containing an alkali treated terpolymer of fatty acid vinyl/α-olefin/maleic anhydride. n CONSTITUTION: The aimed dispersion stabilizer containing a high polymer elec trolyte which is obtained by copolymerizing (B) ≤10C fatty acid vinyl with (C) 10W40C α-olefin and (D) maleic anhydride in molar ratios of the component B:C of 100:0W90:10 and components B+C/component D of 0.8W1.2 in the pres ence of (A) a compound shown by the formula R-(SH) n (R is 1W40C hydrocar bon, etc.; n is 1 or 2) to give a terpolymer and treating the terpolymer with (E) a basic alkaline (earth) metallic compound, ammonia or ≤6C amine, as an active ingredient. n COPYRIGHT: (C)1988,JPO&Japio |