http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S6392710-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D4-04 |
filingDate | 1986-10-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_92a1541b935e7231aa26ad5af184e108 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cc9830f6a01ffbeab4a624cf22613d26 |
publicationDate | 1988-04-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-S6392710-A |
titleOfInvention | Method for melt spinning |
abstract | PURPOSE: To sustain release effect for a long time, and drastically reduce spinneret contamination and eliminate bending, end breakage, etc., by coating the surface of a spinneret with boron nitride as a release agent in subjecting a thermoplastic polymer to melt spinning. n CONSTITUTION: In subjecting a thermoplastic polymer such as polyester, polyamide, etc., to melt spinning, the surface of a spinneret is coated with boron nitride as a release agent in preferably 20W80μm thickness and the boron nitride is baked at 290W320°C for ≥1hr. n COPYRIGHT: (C)1988,JPO&Japio |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-19980080913-A |
priorityDate | 1986-10-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Predicate | Subject |
---|---|
isDiscussedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559551 http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID66227 |
Total number of triples: 14.