http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S6372971-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c11326417f59997dfd0cae39409c42a7 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16J15-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F02F11-00 |
filingDate | 1986-09-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_78b46634ebc0f1cb64969065a4282f19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dc3cd2299cfdcf43d9aee2143f8f8667 |
publicationDate | 1988-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-S6372971-A |
titleOfInvention | Gasket |
abstract | PURPOSE: To enable water resistance and oil resistance properties to be maintained for a long period of time by providing seal pieces on the surfaces of a gasket body piece. n CONSTITUTION: A gasket body piece 1 is made up of a material whose principal component is an expanded graphite. And, on a part or the whole of the surfaces of the body piece 1, at least a kind of seal piece 3 selected from a group consisting of ultraviolet hardened polyurethane acrylate and ultraviolet hardened polysilicon is provided. By this constitution, water resistance and oil resistance properties can be enhanced for a long period of time. n COPYRIGHT: (C)1988,JPO&Japio |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0257764-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H03265762-A |
priorityDate | 1986-09-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 27.