http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S6339969-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2f53aaf6c99bf854b4f9f10f4241e880 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-04 |
filingDate | 1986-08-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d3ac148db69b6232eee859f79dcd6292 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f24bfa1d2ad0dde07c44bfb604108b9f |
publicationDate | 1988-02-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-S6339969-A |
titleOfInvention | Acrylic baking paint composition |
abstract | PURPOSE: To provide the title compsn. having excellent rustproofness and mar resistance, consisting of a specified acrylic resin, a melamine resin and a silane coupling agent-treated glass flake. n CONSTITUTION: 100 pts.wt. resin component consisting of 100 pts.wt. acrylic resin (A) having a glass transition point of 0W15°C and having a soft monomer (e.g., n-butyl acrylate or ethyl acrylate) content of 50W60 wt% and 20W50 pts.wt. melamine resin (B) is blended with 5W30 pts.wt. glass flake (C) having a thickness of 1W10 μm, a length of 5W50 μm an aspect ratio of 5W10 and a surface treated with a silane coupling agent (e.g., γ-methacryloxypropyltrimethoxysilane). n COPYRIGHT: (C)1988,JPO&Japio |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100726980-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H03263473-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0351114-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5066698-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-9116383-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5409994-A |
priorityDate | 1986-08-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |