http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S63285118-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_936cbd88d87d6c8ae7d6992902248355 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-80 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G30-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G23-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C1-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G30-00 |
filingDate | 1987-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9e7d09a1e2be29eb9d42d79c1c817354 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e3f81bab2555c5edaed1b4414241c6eb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_52380902e338aa831540beb2049d2eee http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4efbd19b864282d7be6cd6582a99760e |
publicationDate | 1988-11-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-S63285118-A |
titleOfInvention | Powder of complex electroconductors and its production |
abstract | PURPOSE: To produce a powder of complex electroconductor having hiding effect by coating a powder consisting of titanium dioxide and an inorganic platelet substance with tin oxide containing antimony in the state of solid solution under specific conditions. n CONSTITUTION: A mixture of 10W90pts.wt. of titanium dioxide and the rest pts.wt. of inorganic platelet substance such as mica is made into a powder by the dry or wet method and suspended in water in about 10W500g/l concentration. The aqueous suspension is heated at 50 W about 100°C, and a mixed solution of 100W700g/l of tin chloride and 0.5W180g/l of antimony chloride, containing hydrochloric acid in such an amount as it can prevent the components from being hydrolyzed is added dropwise to the suspension to form electroconductive coating containing 0.1W25wt.% of antimony and the rest of tin oxide substantially so that the weight of the coating layer occupies 5W60% based on the total weight. The coated product is filtered, rinsed, dried, burned at 300W800°C for 30minW4hr and crushed. Thus, a powder of complex electroconductor having high hiding power and electroconductivity is obtained. n COPYRIGHT: (C)1988,JPO&Japio |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H02149424-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2014003179-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H01195606-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014009303-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016520139-A |
priorityDate | 1987-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 38.