http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S6326964-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_460c2d3884b7724541bf93de2a201dfd
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-05
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0568
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-05
filingDate 1986-07-19-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8707e248d05c7f6a38e4feee39944553
publicationDate 1988-02-04-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-S6326964-A
titleOfInvention Nonaqueous electrolyte for polymer battery
abstract PURPOSE:To obtain an electrolyte for polymer battery having sufficient electrolyte concentration and conductivity by forming nonaqueous electrolyte prepared by dissolving lithium salt in a mixed solvent of propylene carbonate and dimethoxyethane in a specific constitution. CONSTITUTION:The conductivity of nonaqueous electrolyte is 1 mS/cm or more at 25 deg.C, and the deposition temperature of lithium salt is 30 deg.C or less, and the concentration of lithium salt is more than 2.5mol/dm<3>. The mixing ratio of propylene carbonate (PC) and dimethoxyethane (DME) is within a range from PC 100% to PC 30%-DME 70%. The concentration of electrolyte is 2.5-4.5 mol/dm<3>.
priorityDate 1986-07-19-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID8071
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419490522
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID7924
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419520276

Total number of triples: 17.