http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S63221133-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 |
filingDate | 1987-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3729f9854473d24a283fd0fb8564c3bf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9abb3e752a68859bb0d03422bb05c42d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_238624252692207675fe90e1a6bb1411 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_563ab6658633a0570f35986d31ae22b4 |
publicationDate | 1988-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-S63221133-A |
titleOfInvention | Biaxially oriented polyester film |
abstract | PURPOSE:To obtain a biaxially oriented polyester film which is flat and excels in lubricity, chipping resistance, etc., by dispersing two kinds of spherical silica particles each of which is specified in the average particle diameter, particle diameter ratio and amount of addition in a polyester. CONSTITUTION:First spherical silica particles having an average particle diameter of 0.6-3mum and a particle diameter ratio (major diameter/minor diameter) of 1-1.2 and second spherical silica particles having an average particle diameter of 0.7-3.1mum and a particle diameter ratio of 1-1.2 are prepared. 0.001-2.5wt.% first spherical silica particles and 0.001-2wt.% second spherical silica particles are dispersed in a polyester (e.g., polyethylene terephthalate). This polyester is formed into a film, which is biaxially oriented to obtain a biaxially oriented polyester film. This film can be suitably used as a base film for videotapes, computer tapes, etc. |
priorityDate | 1987-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Predicate | Subject |
---|---|
isDiscussedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID457707758 http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID24261 |
Total number of triples: 20.