http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S61247746-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_52a65b677bbedbe7bf090dd556a7cc43 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 |
filingDate | 1985-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dadcab455f81c93da976b205dbc32484 |
publicationDate | 1986-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-S61247746-A |
titleOfInvention | Flame-retardant polypropylene composition |
abstract | PURPOSE: To provide the title compsn. which can be readily granulated and is excellent in mechanical strength and flame retardance and suitable for use as a material for electrical insulating material, electrical parts, automobile parts, etc., consisting of PP, Mg(OH) 2 and an org. halogen-contg. flame retarder. n CONSTITUTION: 30W80 wt% PP homopolymer or copolymer of propylene with other olefin (A), 2W25 wt% Mg(OH) 2 (B) having a particle size of 0.1W50μ and a BET specific surface area of 20 m 2 /g or below (optically, its surface being treated with a compd. such as sodium stearate) and 5W40 wt% org. halogen-contg. flame retarder (C) composed of decabromodiphenyl ether and/or dodecachlorododecahydrodimethylbenzocyclooctene are blended in such a proportion that the combined quantity is 100 wt%. If desired, 10W70 wt% (based on the quantity of flame retarder) flame retardand aid composed of an antimocy compd such as Sb 2 O 3 is added thereto. The mixture is mixed in a mixer provided with a high-speed stirrer, fed to a single or twin-screw extruder, melt- kneaded at 200W300°C and extruded to obtain pellets. n COPYRIGHT: (C)1986,JPO&Japio |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-100384948-C http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0568488-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-0149787-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6780914-B2 |
priorityDate | 1985-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 39.