http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S61236849-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cebc9740ef706cde29e885504f274ffa
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L7-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L55-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L55-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-12
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D5-56
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00
filingDate 1985-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f96c819ebeb1fc7d51e3b7dc16b7bf9b
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_69dbe885775997b00614112105459474
publicationDate 1986-10-22-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-S61236849-A
titleOfInvention Impact-resistant thermoplastic resin composition having improved light transmission property and plating
abstract PURPOSE:The titled composition suitable as audio parts, etc., having improved light transmission properties, capable of being plated, obtained by blending a copolymer which is obtained by graft polymerization using rubber with specific particle diameters with a copolymer consisting of an aromatic vinyl and vinyl cyanide. CONSTITUTION:(A) A graft copolymer which is obtained by subjecting A1: 15-65pts.wt. synthetic rubber latex obtained from 50-100wt% 1,3-butadiene and 0-50wt% styrene, having >=60wt% gel content and 0.04-0.1mu average particle diameter and A2: 35-85pts.wt. monomer mixture consisting of 60-90wt% aromatic vinyl monomer and 10-40wt% vinyl cyanide monomer to graft polymerization and has 20-80% graft ratio is blended with (B) a copolymer consisting of B1: 60-90wt% aromatic vinyl monomer and B2: 10-40wt% vinyl cyanide monomer in such a way that the amount of the synthetic rubber is 5-30wt%.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005350566-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H02117942-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0457705-B2
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H03124757-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S62201959-A
priorityDate 1985-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID7845
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID456653168
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419527198
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419547008
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID7855
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID7501

Total number of triples: 32.