http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S6087436-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2261-312
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B5-825
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-73
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L65-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-82
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-66
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-64
filingDate 1983-10-19-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_296f4fe8316dca30c49ed6dd0801116d
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9abb3e752a68859bb0d03422bb05c42d
publicationDate 1985-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-S6087436-A
titleOfInvention Flexible disc for magnetic recording
abstract PURPOSE:To improve dimensional stability by adjusting the coefft. of expansion with temp. and humidity of a biaxially oriented film consisting of poly-p-phenylene sulfide in a specific range. CONSTITUTION:A biaxially oriented film of which >=90mol% consists of poly-p- phenylene sulfide is used as a base in this invention. This film is provided with the expansion characteristics in which the max. coeffts. of expansion with the temp. and humidity at the longitudinal and transverse planes are respectively 9- 35X10<-6> deg.C<-1> and 0-5.0X10<-6>%RH<-1> and the difference between the max. value and min. value of the coefft. of expansion with temp. and humidity are respectively 0-8.0X10<-6> deg.C<-1> and 0-2.0X10<-6>%RH<-1>. The coeffts. of expansion are obtd. by setting adequately film forming conditions. The essential requirement for this film is that >=90mol% thereof consists of the constituting unit of the formula I . Para-halobenzene and alkali sulfide are brought into reaction in a polar solvent as a general method for polymerizing such poly-p-phenylene sulfide.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S6363124-A
priorityDate 1983-10-19-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S5538613-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S59207022-A
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID420033101
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID226417651
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID18938679
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID20508629
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID226423412

Total number of triples: 25.