http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S60208358-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_47cc435e1d443f13180f7766df104d9d http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_80787665b837ed3eb503bbcd27c0043a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K1-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L79-08 |
filingDate | 1984-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0fafbae2d45b109d48ad9a8626519c06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c9f2973eaeaed00bb7a4ae408c3584f0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_084022caca84e255d2cada865828866c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f9bb43982e79cddaf0111a6e00401b54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bcf200d0c5ed825b7062d4a6b796ca22 |
publicationDate | 1985-10-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-S60208358-A |
titleOfInvention | Composite |
abstract | PURPOSE: To obtain a composite resistante to developing deformation and/or cracks caused by thermal stress, thus for use in flexible printing base, by integrating inorganic material and low-thermal expansion polyimide prepared from specific aromatic diamine and aromatic tetracarboxylic acid dianhydride. n CONSTITUTION: The objective composite can be obtained by integrating, either directly or indirectly (i.e. through adhesive or binder), (A) low-thermal expansion polyimide of formula I (Ar 1 is aromatic group of formula II or III; Ar 2 is tetravalent aromatic group of formula IV or V; R is lower alkyl, alkoxyl, etc.; n is 0W4) prepared by reaction at relatively low temperatures in a solution containing, e.g. N-methylpyrrolidone, between an aromatic diamine such as 3,3'-dimethyl benzidine and aromatic tetracarboxylic acid such as pyromellitic acid or its derivative (pref. acid anhydride) to form a polyamic acid varnish followed by heating and (B) inorganic material such as anetal, ceramic (pref. with the surface made coarse, treated with, e.g. silane coupling agent). n COPYRIGHT: (C)1985,JPO&Japio |
priorityDate | 1984-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |