Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_80787665b837ed3eb503bbcd27c0043a |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2045-0015 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2995-0005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2705-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C67-246 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C70-885 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-0013 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K105-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K75-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L31-34 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B7-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C70-88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C67-24 |
filingDate |
1984-03-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_05823b21b61e760ba9bef4913af1f5f1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5db2e81763d03579cc352a6366b8540f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_76ef05ac6f2e198f50114bdb63d6b948 |
publicationDate |
1985-10-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-S60196316-A |
titleOfInvention |
Manufacture of metallic composite solid construction by reactive injection molding |
abstract |
PURPOSE:To manufacture conductive plastics including a fibrous metal and having no jamming of an electromagnetic wave, by dispersing a microcapsule to be obtained by covering a fibrous shape memory alloy deformed into a coillike state with resin is kept dispersed in a cavity. CONSTITUTION:A fibrous shape memory alloy, which has been deformed into a coillike state by applying external force to the same, is made into a microcapsule 6 having appropriate density by covering the alloy with resin, dispersed in the inside of a cavity 5 of a reactive injection mold and both solutions of a polyol stock solution and an isocyanate stock solution are injected from a mixing head 1, which are mixed and solidified. Simultaneously with softening of the resin of the capsule due to heat of reaction the shape memory alloy is extended and a conductive molded article including metallic fiber and having no jamming of an electromagnetic wave is obtained. It is possible to increase the metallic fiber in either a skin layer or a medium layer by making use of a floating or a sinking phenomenon due to density difference among the capsules. There is no abrasion on a kneading screw. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0854026-A1 |
priorityDate |
1984-03-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |