http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S60124616-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6dd74b20fbf2e0ebf10c7bfad4f6c8c5
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-40
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-24
filingDate 1983-12-10-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_37ca29739d177c8d62ed83f02adef9ef
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e32f9566610a26fb8b922a658ebb7538
publicationDate 1985-07-03-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-S60124616-A
titleOfInvention Mixture for semiconductive layer
abstract PURPOSE: A mixture for insulated cable semiconductive layers which can be crosslinked at high temperatures without detriment to releasability in the production of cables, obtained by mixing a polyamide resin comprising a dimer acid with an ethylene copolymer, an epoxy resin, and electroconductive carbon. n CONSTITUTION: A base polymer is prepared by mixing a polyamide resin obtained by polycondensing a dibasic acid component based on the dimer acid of the formula with a diamine with an ethylene/vinyl acetate copolymer and/or an ethylene/acrylate ester copolymer. This base polymer is mixed with an epoxy resin and electroconductive carbon black (e.g., acetylene black) to obtain the purpose mixture of semiconductive layers. When this mixture is used as a material for external semiconductive layers of crosslinked polyolefin insulated cables, these cables can be subjected to corsslinking treatment at a temperature ≥about 300°C without detriment to releasability. n COPYRIGHT: (C)1985,JPO&Japio
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3476898-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111247209-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2020247995-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019081143-A1
priorityDate 1983-12-10-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID6325
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID414862877
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID297
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559542
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559581
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID8121

Total number of triples: 30.