http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S5959783-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_be055db3c1a09879df07379ba969e223 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K5-06 |
filingDate | 1982-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d12f6e7bc7814f2387da0a721fefea0f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_45b94d956a6939e044dde8efe57a66cf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1f6d5245ff145215b9b6b84ff72adfc7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3e50fd54c242b7cd8be531e52d8fee2e |
publicationDate | 1984-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-S5959783-A |
titleOfInvention | Heat storage material |
abstract | PURPOSE: To provide a heat storage material which consists of sodium sulfate decahydrate sodium carbonate decahydrate and urea, has a melting point lower than 25°C and is suitable for heating a passive solar house, etc. n CONSTITUTION: The heat storage material is prepared by blending a mixture of sodium sulfate decahydrate and sodium carbonate decahydrate in a molar ratio of 5:4W2:7, with urea in a molar ratio of 0.95:0.05W0.85:0.15. The composition may contain supercooling inhibitor, thickener, etc. n COPYRIGHT: (C)1984,JPO&Japio |
priorityDate | 1982-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |