http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S5959733-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_13acffa0e4ce30d3be128ccd86b384f6 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01N25-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K9-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-02 |
filingDate | 1982-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cce3ace7330a49e6ce57ef48a5072983 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_268dc5e312b4fe6521b575cc95581136 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6128f21d7f0a819ce814b824cb038cfd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1e3e4c39925cbf7af3fd087ea15cac4b |
publicationDate | 1984-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-S5959733-A |
titleOfInvention | Membrane containing liquid active material and production thereof |
abstract | PURPOSE: To produce a membrane having a liquid active material, which can release the liquid active material at a constant rate over a long period of time, by coating the surface of a support with a soln. obtd. by dissolving a polymer and an active material, which is a liquid at room temp., in a specified org. solvent and then evaporating the solvent. n CONSTITUTION: At least 30wt% polymer (A) such as PS and not more than 70wt% active material (B) (e.g. diazinon), which is a liquid at room temp. and has a solubility of not more than 5pts.wt. per 100pts.wt. polymer at room temp., are dissolved in an org. solvent (e.g. chloroform) in such a proportion as to give a concn. of 10W40wt% in term s of the combined quantity of components A and B, said solvent being capable of dissolving components A and B and being more volatile than component B. The resulting soln. is applied to the surface of a support in a coating thickness of 10W50μ and evaporated by heating at 0W100°C, but at a temp. not higher than the b.p. of the solvent in an atmosphere having humidity of 60% or above to form a polymer layer in which component B in the formh of liquid droplet is enclosed in a lot of micropores which have a pore size of 0.5W10μ and are divided by a partition wall of 0.5W10μ in thickness. n COPYRIGHT: (C)1984,JPO&Japio |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0634428-U http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0591920-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4925730-A |
priorityDate | 1982-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 27.