http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S5943038-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_389de134c635e7b0720da7af149865ee |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-53 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-51 |
filingDate | 1982-09-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9449f4b7583fac1eddb819cb51ce0a0d |
publicationDate | 1984-03-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-S5943038-A |
titleOfInvention | Resin composition having improved electrical conductivity |
abstract | PURPOSE: To provide an electrically conductive resin compsn. having permanent electrical conductivity, by blending metallic copper powder as an electrical conductor and incorporating a specified organophosphorus compd. n CONSTITUTION: An electrically conductive resin compsn. capable of retaining good electrical conductivity over a long period of time is obtd. by incorporating an organophosphorus compd. of formula I (wherein R 1 , R 2 are each halogen, alkyl, cycloalkyl, aralkyl, aryl; R 3 is alkyl, aralkyl, aryl; X is O, S; m, n are each 0W3) such as a compd. of formula II in a resin compsn. contg. metallic copper powder as an electrical conductor blended therewith. When a specified org. titanate compd. such as isopropyltri(di-octyl pyrophosphate)titanate is used together with the organophosphorus compd., the electrical conductivity and its duration can be further improved. n COPYRIGHT: (C)1984,JPO&Japio |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S6471889-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4800661-A |
priorityDate | 1982-09-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 29.