http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S57169050-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f4ff9ddf728a7e1a0b36c9cc38b89ad6
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F3-08
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01H37-58
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F21-08
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F30-16
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F38-08
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F1-15308
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C27-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F1-15316
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C45-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01K7-38
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C27-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01F1-153
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01F1-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01K7-36
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L37-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C45-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C45-02
filingDate 1981-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_52f0ff9530cc4681c9aa7db5851461ce
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_276dd3bf8536892e1a6c76f903174e2d
publicationDate 1982-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-S57169050-A
titleOfInvention Temperature sensitive amorphous magnetic alloy
abstract PURPOSE: To enhance the temp. sensitivity by adding Co, Ni and one or more among P, B, C and Si so as to provide a prescribed composition. n CONSTITUTION: The titled alloy has a composition represented by a formula (Co 1-a Ni a ) 100-z X z (where X is one or more among P, B, C and Si, (a) is 0.2W 0.8 and (z) is 15W20). In the composition ≤5 atomic% Cr may be substituted for the Co. The alloy undergoes a large change in the magnetic permeability due to temp. close to the Curie point, and the temp. range of the change is narrow, so the permeability is changed sharply. The setting temp. is changed to ≤200°C. n COPYRIGHT: (C)1982,JPO&Japio
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0419289-B2
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011518331-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010050386-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011518330-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S63243251-A
priorityDate 1981-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S5669360-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S5739103-A
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419583196
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID104727

Total number of triples: 36.