Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_28c5b8cd65d70d39b7ed1e30c271a218 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M6-164 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M6-16 |
filingDate |
1979-03-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f414b78fb794a9ee886b77090cc48152 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a8116e72f69503ff31efdf77d2adf303 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bdd296fe57d603c5fd5e30651a134d01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_15a7fbc4192f56f40dbfc7eff7f3516e |
publicationDate |
1980-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-S55119363-A |
titleOfInvention |
Nonaqueous electrolyte battery |
abstract |
PURPOSE:To obtain high discharge voltages and voltage stability during discharge, by the use of a mixture solvent of acetonitrile and N,N-dimethylformamide as the solvent to prepare the electrolytic solution in which an inorganic electrolyte is dissolved. CONSTITUTION:A nonaqueous electrolytic solution is prepared by dissolving an inorganic electrolyte into a mixture solvent of acetonitrile and N,N-dimethylformamide at a ratio 95:5-15:85 by volume. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S57105972-A |
priorityDate |
1979-03-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |