http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S54107954-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7acd9416af412b5972feb55a5e652ea2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-20 |
filingDate | 1978-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_06a0e7117e935129978d695bef2ff846 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_81c9c81088886bc6c1aaaa8b0536c212 |
publicationDate | 1979-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-S54107954-A |
titleOfInvention | Amino resin molding material |
abstract | PURPOSE: To reduce volume of an amino resin powder material small, to prevent scattering of the material, and to reduce the loss of the material, by adddng methylpentanetriol and water to the amino resin powder material. n CONSTITUTION: Dried amino resin powder is blended with 0.5W4 wt.% each of a) 3-methylpentane-1,3,5 triol and b) water. The total weight % of a) and b) is not more than 5 wt.%. n EFFECT: The size of a material feed part of molds can be reduced. n COPYRIGHT: (C)1979,JPO&Japio |