http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H1171562-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J109-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J161-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J129-04 |
filingDate | 1998-06-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f8e54551e5952650c91bb0a92e6efd08 |
publicationDate | 1999-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H1171562-A |
titleOfInvention | adhesive |
abstract | (57) [Abstract] [PROBLEMS] To obtain an adhesive having an extremely high initial adhesive strength; In particular, to obtain paper adhesives (for paper tubes, tobacco chip paste, general paper mills, etc.) and woodwork adhesives that require initial adhesive strength. The dispersoid is a (co) polymer comprising at least one monomer unit selected from an ethylenically unsaturated monomer and a diene monomer, and the dispersant is (A) a polyvinyl alcohol-based polymer. In the aqueous emulsion that is united, (B) An adhesive containing an aromatic sulfonic acid alkali metal salt formaldehyde condensate and having a ratio of (A) / (B) of 100 / 0.05 to 100/100 in terms of solid content. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110699016-A |
priorityDate | 1997-07-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 92.