http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H1171454-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_997ed5b3b186e8e8ddd4b0f8685a1d12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G64-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G64-30 |
filingDate | 1997-10-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_018a5b03942234a225c3498cad83c6dc |
publicationDate | 1999-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H1171454-A |
titleOfInvention | Method for producing polycarbonate |
abstract | PROBLEM TO BE SOLVED: To provide a molded product having good moldability, thermal stability and mold corrosivity while maintaining excellent transparency and mechanical properties of a polycarbonate suitable for optical materials, and low birefringence. To provide a method for producing polycarbonate. SOLUTION: In the method for producing a polycarbonate by melt-polycondensing an aromatic dihydroxy compound and a carbonic acid diester, at least 8 0 mol% is (a) 1,1-bis (4-hydroxyphenyl) -3,3,5-trimethylcyclohexane and (b) 4,4 ′-(m-phenylenediisopropylidene) diphenol and / or A method for producing a polycarbonate comprising a specific proportion of 2,2-bis (3-methyl-4-hydroxyphenyl) propane, wherein a specific terminal terminator is added and the terminal is blocked. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4616787-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2021021078-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006193751-A |
priorityDate | 1997-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 269.