Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ded052243c0795fd4fcd4b6428635281 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F212-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F212-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F212-10 |
filingDate |
1997-08-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ed23f9653c3325a775add1387aa72ab0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a04b3973d8cbb923326c6912931b75d5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ddf4a1cb4138f552233803eb89333088 |
publicationDate |
1999-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H1171433-A |
titleOfInvention |
Thermoplastic resin |
abstract |
(57) [Summary] PROBLEM TO BE SOLVED: To provide a compound having a high molecular weight and a molecular weight distribution (Mw / M n) To provide a thermoplastic resin having a wide range and suitable as a modifier for other thermoplastic polymers. SOLUTION: It is obtained by (co) polymerizing at least one selected from the group consisting of an aromatic vinyl compound, a vinyl cyanide compound and another vinyl monomer copolymerizable therewith, and has an intrinsic viscosity of 1 or more. 0.5 dl / g or more, weight average molecular weight / A thermoplastic resin having a number average molecular weight ratio exceeding 3.0. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2012036173-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20180078902-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018124595-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017095532-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10865266-B2 |
priorityDate |
1997-08-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |