http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H1167198-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_61e52b1ec854a16e10c62ce9da02f011 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-32 |
filingDate | 1997-08-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3332bf6496bc775ea83096b2511c75a4 |
publicationDate | 1999-03-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H1167198-A |
titleOfInvention | Method for producing positive electrode active material for alkaline secondary battery, paste-type nickel electrode plate, method for producing the same, and alkaline secondary battery |
abstract | [PROBLEMS] To provide a paste-type nickel electrode for an alkaline secondary battery and a positive electrode active material capable of improving nickel hydroxide utilization and battery capacity of an alkaline secondary battery. SOLUTION: A positive electrode active material composed of nickel hydroxide particles coated with β-cobalt hydroxide is used as a raw material, and is used in an atmosphere substantially free of oxygen. The mixture is heated at a temperature of 0 ° C. to convert the cobalt hydroxide into cobalt oxide, thereby producing a positive electrode active material comprising nickel hydroxide particles coated with cobalt oxide. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100670488-B1 |
priorityDate | 1997-08-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 35.