http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H1160967-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8aa118fbfa85a6e0cc8c13a8afca19ab |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B11-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C25-10 |
filingDate | 1997-08-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_819434d8f4a24b3273894c4be04034b5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7b2f64bdb4143e31c6380151bc7d069f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9f4d0f74593826d1f6d902db947df116 |
publicationDate | 1999-03-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H1160967-A |
titleOfInvention | Sheet molding compound |
abstract | PROBLEM TO BE SOLVED: To prevent the generation of static electricity when cutting a glass roving, to reduce the boiling resistance of the FRP molded product, and to prevent the coloration of the glass fiber from impairing the color tone of the sheet molding. The purpose is to provide the compound. SOLUTION: Lauryl dimethyl ethyl ammonium ethyl sulfate is used as an active ingredient in an amount of 0.1% as an antistatic agent. 3% by weight, 0.2% by weight of γ-methacryloxypropyltrimethoxysilane as a coupling agent, 0.1% by weight of a cationic surfactant as a lubricant, and 10% by weight of a vinyl acetate emulsion as a film former The preparation was prepared. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014058436-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017186731-A |
priorityDate | 1997-08-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 30.