abstract |
(57) [Summary] Next steps: (a) Forming a substrate 1 that is substantially transparent to radiation of wavelength λ, and forming a substrate 1 on one surface 1 a of a metal partitioned into an array of islands 5 (B) irradiating a laser beam 7 having a wavelength of λ onto the island through the substrate 1, whereby the island 5 is quickly melted and the island 5 is melted and dropped. And detaching it from the substrate 1 in the shape of No. 9. In one preferred embodiment of the method of the invention, the molten droplet 9 is "shot" on the target substrate before solidification. |