http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H11350323-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2cb72657cf0479385a9b5e655af1e16f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H1-544 |
filingDate | 1998-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d15b8f2b57fa3369d6c95aeb7ececed7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c9e0511b8f6f74e21701099617a63403 |
publicationDate | 1999-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H11350323-A |
titleOfInvention | Spunbond nonwoven fabric and skin patch |
abstract | (57) [Problem] To provide a spunbonded nonwoven fabric and a skin patch which are excellent in texture, stretchability and continuous productivity. SOLUTION: Ethylene which satisfies the following (A) to (D) A spunbond nonwoven fabric and a skin patch formed using an α-olefin copolymer material. (A) Density (ρ) is 0.86-0.9 g / cm 3 (A) The standard deviation of the average elution temperature except for 0 ° C., which is obtained by a temperature rising fractionation method, is 6 ° C. or more. 100 (g / 10 min) (d) Molecular weight distribution (Mw / Mn) is 3.0 or less |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007321291-A |
priorityDate | 1998-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 21.