abstract |
(57) [Problem] To provide a propylene-based resin composition capable of easily producing a molded article having an excellent balance between rigidity and impact resistance (particularly low-temperature impact resistance). SOLUTION: The propylene unit has 100 to 80 mol%, When the constitutional unit derived from the comonomer is present in an amount of 0 to 20 mol%, the MFR is 0.1 to 200 g / 10 min, the average elution temperature is in the range of 75 to 120 ° C., and the elution dispersity is 9 or less. A propylene-based resin composition is obtained by mixing a glass fiber, an unsaturated carboxylic acid-modified polypropylene, and optionally an elastomer and / or a Ziegler-based polypropylene with a certain propylene-based polymer. |