Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L9-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B37-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-08 |
filingDate |
1998-05-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_51b6a5ea4f32915c02c0d9e1db6edc53 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5dec0e448ad3cf81c4dbf413a2f9c864 |
publicationDate |
1999-11-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H11320671-A |
titleOfInvention |
Method and apparatus for producing stretched film |
abstract |
PROBLEM TO BE SOLVED: To provide a method and an apparatus for producing a plastic film, which improve the productivity of a coated film by improving a drying step of an aqueous coating agent. SOLUTION: In a method for producing a plastic sheet having a step of applying an aqueous coating agent on at least one surface of a traveling plastic film, after the applying step, the coating agent is dried using a near-infrared radiation heater and heated air. A method for producing a plastic film, which comprises a step, and an apparatus therefor. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2014163175-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018047695-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-0185363-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4819282-B2 |
priorityDate |
1998-05-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |