http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H11302463-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1d29f7ac2c7f9be9f7dae1a83bbb5c92 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-00 |
filingDate | 1998-04-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7fe05d910f3e54a73a0571d1e65b4424 |
publicationDate | 1999-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H11302463-A |
titleOfInvention | Soft polyolefin resin composition |
abstract | (57) [Summary] [Problem] By combining a specific fibrous filler and / or a plate-like filler with a specific soft polyolefin, at the time of compressive deformation, a balance between compressive stress and compressive stress relaxation, recyclability and harmfulness. An object of the present invention is to provide a soft polyolefin resin composition excellent in environmental protection such as generation of combustion gas. (A) fractionated by a temperature rising elution fractionation method 100 parts by weight of a soft polyolefin resin having an elution component of 10 to 90 wt% at 40 to 30 ° C., (B) a fibrous filler having an average fiber diameter of 0.1 to 2 μm and an aspect ratio of 5 to 100 and / or an average particle diameter. It is a soft polyolefin resin composition obtained from 1 to 300 parts by weight of a plate-like filler having an aspect ratio of 0.5 to 10 µm and an aspect ratio of 5 to 100. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014196421-A |
priorityDate | 1998-04-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 104.