http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H11300891-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1beb91e1aec5bce64017e33d87331702 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-80 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B25-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D30-02 |
filingDate | 1998-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c837498a2bee3fdd728abf573e1a2d25 |
publicationDate | 1999-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H11300891-A |
titleOfInvention | Laminated sheets and flexible containers |
abstract | (57) [Problem] To provide a laminated sheet for a flexible container excellent in physical properties, ozone resistance and chemical resistance. By washing treatment with hot water or steam, To provide a flexible container which can maintain desired physical properties and can be reused after the cleaning treatment. SOLUTION: In the laminated sheet of the present invention, a crosslinked rubber sheet 2A is formed on one surface of a base fabric 1, a crosslinked rubber sheet 2B is formed on the other surface of the base fabric 1, and the surface of the crosslinked rubber sheet 2B is formed. A resin film 3 is formed so as to cover, and each of the crosslinked rubber sheets formed on both sides of the base fabric 1 contains hydrogenated nitrile rubber. In the flexible container of the present invention, the laminated sheet is formed into a bag shape, and the inner surface that comes into contact with the liquid substance is formed of a resin film. |