http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H11286090-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-189 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-08 |
filingDate | 1998-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2fe2a602a4e134c47e63cab8faae9b77 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2826f096e546745ccc5f3cec94d2df55 |
publicationDate | 1999-10-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H11286090-A |
titleOfInvention | Polyester film for metal plate lamination processing |
abstract | (57) [Abstract] [Problem] To provide a polyester film for metal plate laminating processing which is excellent in formability such as deep drawing, heat resistance, retort resistance, and has improved impact resistance, taste retention and fragrance retention. provide. SOLUTION: A layer (A) composed of copolymerized polyethylene terephthalate and a layer (B) composed of copolymerized polyester. Wherein the glass transition temperature (Tg A ) of the polymer constituting the layer (A) and the peak temperature of the maximum loss modulus (Te) of the film are represented by the following formulas (1) and (Te). 2. A polyester film for laminating and processing a metal plate, which satisfies (2) and further has a polymer melting point of the layer (A) higher than that of the layer (B), and a difference of 2 ° C. or more. Tg A ≧ 78 (1) Te−Tg A ≦ 30 (2) (where Tg A is the glass transition temperature (° C.) of the polyester constituting the copolymerized polyester layer (A) in DSC measurement, and Te is the film Is the highest peak temperature (° C.) of the loss elastic modulus.) |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008162221-A |
priorityDate | 1998-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 31.