http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H11276638-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dd44e4633eb2354495cc5750ff490ca2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A63B37-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-06 |
filingDate | 1998-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ffa3202a0e5b6f416c57f02449a7221d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_02e89d11f41a90d32f0c2860733a9aa3 |
publicationDate | 1999-10-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H11276638-A |
titleOfInvention | Golf ball material |
abstract | (57) [Problem] To provide a golf ball material having excellent rebound resilience, durability, excellent ball control properties, easy spin, and excellent shot feeling. SOLUTION: (A) an ethylene copolymer ionomer (preferably having a Shore D hardness of 55 or more) ... 30 to 9 Part or all of 5 parts by weight and (B) a copolymer of ethylene and an α-olefin having 4 or more carbon atoms is graft-modified with an unsaturated dicarboxylic anhydride and has a density of 850 to 91. 0 kg / m 3 , especially weight average molecular weight / number average molecular weight of 3 The following graft copolymer: A golf ball material comprising a resin composition in an amount of 70 to 5 parts by weight. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8450419-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008023332-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10316174-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9637625-B2 |
priorityDate | 1998-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 49.