http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H1124275-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_13aa7b32ae00ed83af7dfaa0b6a1f7c2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-095 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-028 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-00 |
filingDate | 1997-07-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b5e6672706312d71bd3238d69567d229 |
publicationDate | 1999-01-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H1124275-A |
titleOfInvention | Method for producing photosensitive lithographic printing plate and photosensitive lithographic printing plate |
abstract | PROBLEM TO BE SOLVED: To provide a photosensitive lithographic printing plate in which image defects due to a ballpoint pen trace drawn on the surface of a photosensitive layer are improved, and which have good developability, printing durability and chemical resistance, and a method for producing the same ( In particular, the above effects can be obtained even if the photosensitive layer is made thinner). A photosensitive lithographic printing plate comprising a support and a plurality of coating layers including a photosensitive layer containing a compound capable of generating an acid or a radical by light, actinic radiation or an electron beam. Wherein the uppermost layer of the coating layer contains a filler having an average particle size smaller than the dry thickness of the uppermost layer, the dry thickness is 0.5 μm or less, and the uppermost layer And at least one of the other coating layers is applied by a wet-on-wet method. In the photosensitive lithographic printing plate (a), the average surface roughness (Ra), the 10-point average roughness (Rz), and the maximum surface roughness (Rmax) of the uppermost layer are Rz / Ra. A photosensitive lithographic printing plate satisfying ≦ 8 and Rmax / Ra ≦ 14. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6564712-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008158007-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004310076-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009282512-A |
priorityDate | 1997-07-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 181.