http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H11233101-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8fb9f44db08d1c42a53f3d28eaae416f |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-139 |
filingDate | 1998-02-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e75f3a98a151a5509054a0faaa3b953b |
publicationDate | 1999-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H11233101-A |
titleOfInvention | Negative electrode for non-aqueous secondary batteries |
abstract | (57) [Summary] [PROBLEMS] To provide a high capacity and lightweight non-aqueous secondary battery. SOLUTION: In a non-aqueous secondary battery having a positive electrode and a negative electrode containing an active material capable of inserting and releasing lithium ions, A conductive thin film portion made of a conductive metal is formed on one or both surfaces of the rectangular film containing the negative electrode active material by using either the electrolytic plating method or the electroless plating method, and the conductive thin film portion of the rectangular film is formed. Two or more rectangular films are stacked facing each other to form a negative electrode. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4546740-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014035886-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005197096-A |
priorityDate | 1998-02-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 45.