http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H11223719-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K26-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-382 |
filingDate | 1998-02-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_57cf3b4b9e1271591df2b12fc6d59014 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eae9191139404f339b555ee80e5cd8e6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ddb15b3ad3fdd66baacf53abd953d76c |
publicationDate | 1999-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H11223719-A |
titleOfInvention | Method of forming colored pattern and method of manufacturing color filter |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a color filter in which pixels of a plurality of hues are formed in a pattern on a substrate by a laser beam irradiation method using a coloring composition. An object of the present invention is to provide a method of manufacturing a color filter which is excellent in color quality without light leakage at a side portion of each pixel and which can improve a yield in a liquid crystal cell manufacturing process. SOLUTION: A colored coating film on a substrate is irradiated with a laser beam in a pattern to evaporate a portion to be irradiated, In the method of forming a colored pattern, The colored coating film is irradiated through a photomask having a predetermined opening pattern and an imaging lens, and at that time, the irradiation energy density E of the laser beam, the true imaging position of the imaging lens, and the surface of the colored coating film are compared. A method for forming a colored pattern in which the gap d is adjusted so that the width a of the slope at the cross-sectional end of each colored pattern to be formed is within a range of 5 μm or less. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009069841-A |
priorityDate | 1998-02-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 79.