Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bcdb7859d196574348806c539e0e92d6 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-5419 |
filingDate |
1998-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_481a402d83dec8a0419a4dd757d01e82 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4443206438edb9e7d2213c2e18180fa6 |
publicationDate |
1999-08-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H11217467-A |
titleOfInvention |
Non-halogen flame-retardant resin composition |
abstract |
PROBLEM TO BE SOLVED: To provide a non-halogen flame-retardant resin composition having excellent mechanical properties, which is excellent in both tensile strength and elongation, as well as having excellent flame retardancy. provide. SOLUTION: In the flame-retardant resin composition obtained by mixing a metal hydrate and a silane crosslinking agent with an olefin resin, a metal hydrate surface-treated with silane is used as the metal hydrate. Flame retardant resin composition. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016541006-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100341112-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6706409-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1170116-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006225568-A |
priorityDate |
1998-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |