http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H11202438-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_13aa7b32ae00ed83af7dfaa0b6a1f7c2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-35 |
filingDate | 1998-01-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b0441e288f6d593e2070ee52b737049b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_78f1d8a8d0fc648c19becda585721267 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2f27ffbdd4b8c758bd9c8a4f3b4975df |
publicationDate | 1999-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H11202438-A |
titleOfInvention | Silver halide photographic material and processing method thereof |
abstract | (57) [Summary] [Problem] To provide a silver halide photographic light-sensitive material which is excellent in roller mark resistance, and which can provide a cool black tone and easy-to-see silver images which can be processed quickly. SOLUTION: In a silver halide photographic material having at least one silver halide emulsion layer on a support and at least one non-photosensitive hydrophilic colloid layer thereon, the degree of swelling of the emulsion layer immediately after development is reduced. Wherein the ratio of the total film thickness immediately after development to the total film thickness of the silver halide photographic material before processing is smaller than the swelling degree of the non-photosensitive hydrophilic colloid layer is 1.2 to 3. Silver halide photographic light-sensitive material. |
priorityDate | 1998-01-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |