http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H11199727-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_47cc435e1d443f13180f7766df104d9d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L55-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 |
filingDate | 1998-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_737d4f04eb3b4c8fca3f078f0e4e7437 |
publicationDate | 1999-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H11199727-A |
titleOfInvention | Styrene resin composition for vibration welding |
abstract | (57) [Summary] [Problem] When an acrylic resin is joined to a styrene resin composition for vibration welding by vibration welding, the collapse of burrs and the generation of powdery materials are reduced, and an excellent joint surface appearance is obtained. Provided is a styrene-based resin composition which can be obtained by vibration welding. SOLUTION: In the styrene resin composition for vibration welding used when the acrylic resin is subjected to vibration welding, the styrene resin composition for vibration welding contains a rubber-modified styrene resin, and the styrene resin for vibration welding is used. A of the composition The flexural modulus according to STM-D256 is set to a value of 2.5 GPa or more. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016188292-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002322340-A |
priorityDate | 1998-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 47.