Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a7de2addb5b81a5205407e4286cba7fb |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B14-24 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B111-40 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E04B2-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B38-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B14-24 |
filingDate |
1997-12-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a443760e473a1f911a01359914db4c79 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3ebb6b42ec986c921dbd902d01f26d05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_38481a69f13945bf54b62b8b0a651709 |
publicationDate |
1999-07-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H11189479-A |
titleOfInvention |
Lightweight block |
abstract |
(57) [Summary] [Problem] A lightweight block. SOLUTION: The lightweight block of the present invention is made of a cement composition mixed with a lightweight aggregate and having a specific gravity of 1 or less, and an inorganic aggregate such as a hollow glass sphere is suitably used as the lightweight aggregate. . Also, if the large-diameter recycled glass foam and the small-diameter shirasu balloon are used in an appropriate mixing ratio, the filling rate of the aggregate increases, and the engagement of the aggregate increases, so that both the demolding rate and the strength increase. It becomes suitable. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102206065-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103011705-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009502469-A |
priorityDate |
1997-12-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |