http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H11176431-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_61e52b1ec854a16e10c62ce9da02f011 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-30 |
filingDate | 1997-12-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3332bf6496bc775ea83096b2511c75a4 |
publicationDate | 1999-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H11176431-A |
titleOfInvention | Manufacturing method of paste-type nickel electrode, paste-type nickel electrode and alkaline secondary battery |
abstract | (57) [Summary] [Object] To provide a paste-type nickel electrode with improved utilization and high-temperature charge acceptability. A three-dimensional porous current collector is filled with a powder of nickel hydroxide particles coated with β-cobalt hydroxide and heated and oxidized in air to form the β-cobalt hydroxide film in oxywater. The coating is made of cobalt oxide and cobalt tetroxide. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9276258-B2 |
priorityDate | 1997-12-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 45.