Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5128cfc84a0fb189fceb3cd240c44493 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K101-12 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-49 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C47-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-215 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C47-82 |
filingDate |
1997-12-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1dd55448cf5c0d276a3b6ac675554f80 |
publicationDate |
1999-06-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H11172009-A |
titleOfInvention |
Method for producing liquid material-containing resin composition |
abstract |
PROBLEM TO BE SOLVED: To provide a method for producing a liquid substance-containing resin composition having excellent appearance, light resistance and mechanical properties by adding a liquid substance to a thermoplastic resin by a special method. SOLUTION: In a method for producing a resin composition containing (A) a thermoplastic resin and (B) a liquid substance having a liquid state in a temperature range of 25 ° C. to 300 ° C., (B) first becomes a liquid state. (A) and (B) are mixed to lower the glass transition temperature (Tg) of (A) at a temperature selected from the temperature range of from 300 ° C. to 300 ° C .; A method for producing a resin composition containing a liquid substance, which comprises melt-extruding at 300 ° C. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4518601-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4589890-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001131392-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2722699-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2722699-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20170066386-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2012173190-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2004033538-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004269885-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007171894-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010077449-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2012173190-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003020343-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003048994-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002114875-A |
priorityDate |
1997-12-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |