abstract |
PROBLEM TO BE SOLVED: To provide a thermoplastic molding material containing polyarylene ether and polyarylene sulfide and avoiding the disadvantages of known molding materials. SOLUTION: A total of 100% by weight of a thermoplastic molding material is used. A: 5-94% by weight of at least one polyarylene ether as component A, b: at least one polyarylene sulfide 4 as component B, based on the total weight of components A to D and, if present, E ~ 93% by weight, c: 1 to 20% by weight of at least one carboxyl-containing polyarylene ether as component C, d: Impact modified rubber 1 having at least one functional group capable of reacting with a carboxyl group as component D -20% by weight, e: Other additives as component E 0-50 % By weight. |