http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H1115088-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C2001-0056 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C2001-03535 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C2001-0055 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C2200-43 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C2001-0357 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-0051 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-015 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-005 |
filingDate | 1997-06-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fbcf2f9ed3f230c1f1728110f0d9446f |
publicationDate | 1999-01-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H1115088-A |
titleOfInvention | Method for producing silver halide photographic emulsion, silver halide photographic emulsion using the same, and silver halide photographic light-sensitive material containing the emulsion |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a silver halide photographic emulsion having high sensitivity and little change in photographic properties due to stress, a silver halide photographic emulsion using the same and a silver halide photographic light-sensitive material containing the emulsion. To provide. SOLUTION: Tabular grains having an aspect ratio of 3.0 or more and an equivalent circle diameter of 1.4 µm or more occupy 50% or more of the total projected area of silver halide. It consists essentially of a host tabular grain forming step (step a), a step of adding an emulsion containing poorly soluble silver halide grains (step b), and an outermost shell layer forming step (step c), and is consumed in step a. (C Ag ) and the amount of silver (S Ag ) consumed in step b and step c are (I) Formula: S Ag / C Ag = {R 3 / (R−d) 3 } −1 (d is 0 <d ≦ 0.15, and R represents the equivalent spherical diameter of the final particles. A method for producing a silver halide photographic emulsion, characterized by the following: |
priorityDate | 1997-06-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links