http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H11140120-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F16-06 |
filingDate | 1997-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7db27e79dcc1471da6edf869fbed8b85 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f1d6062447d4cc26a4cc5be5d05b4cdf |
publicationDate | 1999-05-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H11140120-A |
titleOfInvention | Manufacturing method of membrane |
abstract | PROBLEM TO BE SOLVED: To provide a novel polyvinyl which has characteristics of a conventional film made of a polyvinyl alcohol polymer such as high strength, transparency and oil resistance, and also has excellent heat resistance, water resistance and wet heat resistance. Provided is a film comprising an alcohol-based polymer. SOLUTION: When producing a film made of a polyvinyl alcohol-based polymer, a polyhydric ethanol compound having two or more ethanol structures adjacent to an electron-withdrawing group is added to the polyvinyl alcohol-based polymer at a ratio of 0.1 to 0.1. 05 A method for producing a film, characterized in that the polymer is crosslinked by a heat treatment after containing or adhering to 20 mol%. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-03072653-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-1294198-C http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7534829-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007191713-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100906949-B1 |
priorityDate | 1997-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |